Page 199 - Mirjam-Theelen-Degradation-of-CIGS-solar-cells
P. 199
Degradation mechanisms of the aluminium doped zinc oxide front contact


(a)
Transmittance H 2O/O 2
80
Optical parameters (%) 60 Absorbance



40

20
Absorbance
0
500 1000 1500 2000
Wavelength (nm)

(b)
Transmittance H 2O
80 Absorbance
Optical properties (%) 40 Reflectance

60


20

0
500 1000 1500 2000
Wavelength (nm)


(c)
Transmittance H 2O/air
80 Absorbance
Optical parameters (%) 60



40

20
Reflectance
0
500 1000 1500 2000
Wavelength (nm)
Figure 6.16
Optical properties before (red) and after 310 hours exposure to various conditions (blue) which are (a) H 2 O/O 2 (b) non-
purged H 2 O (c) H 2 O/air.



197
   194   195   196   197   198   199   200   201   202   203   204